Quote:
Originally Posted by deadbodyman View Post
John ,I imagine you keep that car inside and totally clean only driving it on weekends and such...I think the sun has a lot to do with that bubbling and would have shown up much earlier if it was kept outside or was a DD..
.its definately an adheasion problem and most likely caused from the rust mort whether its the product itself or (god forbid) user error is the question...but being that its in the reveil tends to make me think there was some excess left in there that was missed from sanding.
I tend to think this my fault. I posted pictures on the PPG Deltron epoxy thread. Take a look and see what you think. I personally think it may be a 2 fold problem. Metal needs more tooth and acid needs to be neutralized.