Thank you all for consideration.
Here I got : sbc 350 STD to be bored to 0.040 (never decked), cast crank , Probe FPS Flat top -4 cc, forged rods (5.7") , 64 cc aluminum heads (190 cc runners, 2.02/1.90), 1.5 ratio roller type rockers , Howard Hyd. 110041 cam (Duration :235 Ex, 225 In - Valve lift:.488 Ex ,.465 In. - 110 LC - 106 Intake C/L -Intake closes @38.5 deg. ABDC ), Head Gasket Fel pro 1003 (4.166 Dia, 0.041 compressed thickness)
Not sure or insufficient information about quench distance stuff or decking.
Any comment or help is really appreciated.
|