Spi Sealer/deltron Basecoat/spi Clearcoat?
I repainted a 1994 2 DR yukon which has fender flares. I removed the fender flares to repaint the vehicle. After painting and waiting approximately 7 to 10 days I reinstalled the fender flares and the paint crinkled along the edge of the fender flare. Really no other problems to speak of with the paint job. Paint does seem to chip easy from rocks and such but no paint lifting etc.
It appears there where some bonding issues with thePPG BC and SPI sealer. The clear coat was wet sanded and buffed with no problems although it never appeared to shine. Planning to do some scratch repair on the vehicle from my teenager. Just wondering if anyone had experience this before or had any thoughts on this?
Thanks
|