Well, glass smooth may be the wrong choice of words. All over the forum I see laying K-36 over 180 grit is acceptable, I'm way past that. Over the finish I end up with will be more DPLF then the K-36; I'll resand with 5 or 600 before base coat.

Thanks for the input, I'm open minded and appreciate it all.
__________________
I'm the one your momma never told you about...

Semper Fi


To view links or images in signatures your post count must be 10 or greater. You currently have 0 posts.



To view links or images in signatures your post count must be 10 or greater. You currently have 0 posts.
Reply With Quote