I am in the process of duing bodywork on my car and when i get done i cover everything up with a self etching and sealing primer but it wont stick at all it looks like the primer itself is shrinking, if any body has any idea help me, the rain has started and i need to get the bare metal covered up quik thanks guys
:confused: <img src="graemlins/crash.gif" border="0" alt="[crash]" /> :(
 

· Registered
Joined
·
37 Posts
Discussion Starter · #5 ·
I have scuffed the surface with 80grit paper, i cleened it with prepsol and air temp is about 60degrees and surface temp was probably 50-55?
i guess my main prob was the temp right?