After glass beading the rust before I sent my grill pieces for chroming I found holes. I would like to make a repair by brazing before I take it to be plated but I'm not sure how to start. How should I clean the metal before brazing? I found 41willys's post in the archives but it left out some steps. How about some more advice 41willys. Should I consider mig welding instead? Need advice. Thanks Jesse ( The chrome is still there, it is the only thing left before the rust is through)